Got a question for you die attach gurus. We are currently using boards with
electroless gold finish. We have a supplier that has sent in boards with
electro-plated gold and we are seeing our die shear's going down. I would
expect to see some decrease in die shears but we are seeing in some cases
50% reduction. Any body out there doing both types of gold finishes and if
so are your parameters and things like flux the same for both?
Thanks
Scott B. Westheimer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------