Hi Chuck,
Really!? To tell you the truth I had no idea this would be the cause, I was more focused, as I said, on the flux residue! How did you realize it was the solder mask?
Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing
941 Route 38 Owego, NY 13827
Phone: (607) 687-7669 x349
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chuck Brummer
Sent: Tuesday, April 11, 2006 2:13 PM
To: [log in to unmask]
Subject: Re: [TN] White Residue in the oven
I bet it comes from the solder mask. I use Photo Coverlay on our flexes
and get white fungus like stuff in the exhaust duct and around the door of
my cure oven.
The good news is an industrial hygienist checked it out and found nothing
dangerous.
Chuck Brummer
3M Manufacturing Engineer
8357 Canoga Ave.
Canoga Park, CA 91304-2605
(818) 734-4930
"Kane, Amol (349)" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
04/11/2006 08:46 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Kane, Amol (349)" <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] White Residue in the oven
Hi Technetters,
I have a white residue coating all over my reflow oven innards (almost
looks like white fungus). How can I absolutely be certain that it's flux
and not anything else?are there any tests available for this? I am
planning to check the oven exhaust for correct air flow rates.....anything
else I should be looking out for?. We are using a water soluble halide
free flux and SnPb solder
Thanks in advance
Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing
941 Route 38 Owego, NY 13827
Phone: (607) 687-7669 x349
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|