TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Date:
Tue, 11 Apr 2006 12:37:50 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jason Gregory <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Subject:
From:
Jason Gregory <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
Innova Electronics, LP
MIME-Version:
1.0
Parts/Attachments:
text/plain (142 lines)
Hi Ramon,

Pros:
-Ability to process problematic high temp boards (thicker than .063", high
layer counts, etc.) and not have to jack with as many variables as in
convection or IR
-Excellent thermal equilibrium across the assembly and not having to worry
about shadowing or thermal thieving
-Probing your board to determine preheat and then knowing your peak area's
temp already and looking through a little window to observe reflow and
giving an extra 15 or 20 seconds over for wetting

Cons:
-Fluid is expensive and if you have excess dragout, you will notice
financially. Fluid is about $1000/gallon
-Higher than usual expectations for tombstoning if your board design is a
little lopsided (heavy ground planes connected to one side of passives) or
if your process is a little off.
-Machine is a booger to clean


Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)594-0602 cell
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Tuesday, April 11, 2006 11:36 AM
To: [log in to unmask]
Subject: Re: [TN] RD Technologies Vapor Phase Users

        Hi Jason:
                   I believe that Vapor phase has a lot of good merits.
Could you share your experience with the machine? Pros and Cons.
        Regards,
        Ramon


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Gregory
Sent: Tuesday, April 11, 2006 12:13 PM
To: [log in to unmask]
Subject: Re: [TN] RD Technologies Vapor Phase Users

Hello Steve,

We have a RD here and we use Galden HS-260


Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)594-0602 cell
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, April 11, 2006 10:33 AM
To: [log in to unmask]
Subject: [TN] RD Technologies Vapor Phase Users

Mornin' All!

I've just got the opportunity to work with a new vapor phase reflow system
here at my new position. It's a RD Technologies RD3 with a vapor recovery
system. We're in the process of hooking it up, we haven't yet started it up.

I worked with a vapor phase many years ago (1988), and this system is much
nicer than what I remember about the system I worked with in the past.

I was wondering if there are any RD Technologies users out there that have
any "words of wisdom" that they might share with me about the system I'm
that going to be working with. BTW, we're going to using Galden heat
transfer fluids.

Kind regards,

-Steve Gregory-
Senior Production Engineer
OAI Electronics
6960 East 12th Street
Tulsa, Oklahoma 74112

(918) 836-0507
(918) 706-2779 CELL
(918) 836-0184 FAX

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2