Agreed. Many customers look favorably on rework methods called out in
7711, but do not want to allow "generalized" repairs specified in 7721,
and have the difficulty of not being able to allow the one without the
other because the document is combined. Many companies have their own
repair procedures that specify a particular epoxy, wire or other
materials/methods, such as low-outgassing materials for space use.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(AZ75)
Sent: Thursday, April 06, 2006 12:28 PM
To: [log in to unmask]
Subject: Re: [TN] relationship between J-STD-001 and IPC 7711/7721: need
your help.
This is one area where I disagree with the IPC approach. IPC 7711 and
IPC 7721 should have never been put together. There was an expectation
that things that were done in 7711 would meet acceptance criteria
established in J-STD-001 and 610 for class 3. 7721 reflects
methodologies that exist, but are not necessarily compliant with
anything, unless you say so in your own documentation.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of prasad godavarti
Sent: Thursday, April 06, 2006 7:38 AM
To: [log in to unmask]
Subject: [TN] relationship between J-STD-001 and IPC 7711/7721: need
your help.
In a nutshell here is where i need some help:
we call out and enforce J-STD-001, Class 3 on our assembly drawings.
Very often we do repair/rework on these assemblies and we do not seem to
have a clear link between IPC 7711 and IPC 7721 wherein the how-to's and
what to control are listed and J-STD-001, Class3. The only words that
address repair/rework in
J-STD-001 have to do with the acceptance criteria for such operations.
Ques:
1. I am reading this correctly?
2. How do i ensure that the repair and rework procedures and the skill
sets are adequate? do I need to explicitly state in on the drawing the
need for repair and rework per IPC 771 and IPC 7721?
3. If i do not state that then is the compliance to
J-std-001 violated?
Thanks
Prasad Godavarti
__________________________________________________
Do You Yahoo!?
Tired of spam? Yahoo! Mail has the best spam protection around
http://mail.yahoo.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|