TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jason Gregory <[log in to unmask]>
Date:
Sun, 2 Apr 2006 20:38:43 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="US-ASCII"
From:
Richard Kraszewski <[log in to unmask]>
Parts/Attachments:
text/plain (192 lines)
Problem is this doesn't do much for me if I'm using SAC305.

Rich K / KEDS

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Gregory
Sent: Thursday, March 30, 2006 4:41 PM
To: [log in to unmask]
Subject: Re: [TN] Maximum Contamination Levels in Solder

Joel,

Sorry I mis-quoted you, I apologize.

Our lab uses J-STD-001 specs and they list as follows:

Tin             94.5 - 97.5%
Arsenic         0.030% max
Antimony        0.500% max
Gold            0.200% max
Iron            0.020% max
Nickel          0.010% max
Bismuth         0.250% max
Aluminum        0.005% max
Copper          0.300% max
Silver          3.750 - 4.250 %
Zinc            0.005% max
Cadmium 0.005% max
Indium          0.100% max
Sulphur         0.005% max
Phosphorous     0.010% max
Lead            balance


Hope this helps


Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)594-0602 cell
[log in to unmask]

-----Original Message-----
From: Joel Mearig [mailto:[log in to unmask]]
Sent: Thursday, March 30, 2006 3:23 PM
To: 'TechNet E-Mail Forum'; 'Jason Gregory'
Subject: RE: [TN] Maximum Contamination Levels in Solder

Jason,
I can't find where I used the term "then one of the alloy components".
When
I say "if not one of the alloy components" the test looks like this.

Copper specification is 0.3wt%. I always fail that spec because I am
using a
0.5% copper alloy. So the lab says it is fine because the metal is "one
of
the alloy components". What they don't tell me is at what level the
copper
content is really too high and I need to change the solder in the pot.
Similarly I also fail the silver every time. At the moment I am
deciding, on
my own, when the other metal levels are "out of spec" and am looking for
someone to validate my numbers by providing an "industry standard"
specification for lead-free tests.

If you could provide the SN96.5 specification your lab uses that would
provide information that I can use to validate my numbers assuming it is
a
96.5Sn, 3.0Ag, 0.5Cu alloy.     Thanks          Joel

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Gregory
Sent: Thursday, March 30, 2006 12:03 PM
To: [log in to unmask]
Subject: Re: [TN] Maximum Contamination Levels in Solder

I don't understand what you mean by the "then one of the alloy
components"
statement. However, if your lab is testing by Sn/Pb standards, then you
should fail the high amount of tin every time.  My lab tests with an
SN96.5
spec. What was funny is that one test we "failed" or we were out of spec
on
the SN content, but they had inadvertently selected SN96 for the test
instead of SN96.5. Even that minute change threw us off (they corrected
it
though), so I think testing to Sn/Pb would make you fail every time.



Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)594-0602 cell
[log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joel Mearig
Sent: Thursday, March 30, 2006 11:14 AM
To: [log in to unmask]
Subject: [TN] Maximum Contamination Levels in Solder

I have the solder tested in my solder pots on a regular basis. However,
the
testing lab continues to provide results based on Sn/Pb standards even
though the solder is lead-free. The lab clarifies the results with the
"if
not one of the alloy components" statement.



I was wondering if there was a different contamination levels chart for
lead-free solder that I could get my testing lab to use.



Any help would be greatly appreciated.



Joel Mearig




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2