TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 26 Apr 2006 16:02:59 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Jeffrey Bush <[log in to unmask]>
Parts/Attachments:
text/plain (79 lines)
I think a gap exists in understanding what I am saying.  The designer
should specify what the finished dimensions are for all factors and let
the PCB house get there based on their specific process capabilities.
Size, circuit geometry, aspect ratio, etc. all have an impact on the
resulting plating deposit, which is further complicated by many
differing plating processes equipments and techniques.  This has nothing
to do with the function of the board and the need for the PCB house to
understand this.  If the desired finished result is articulated on the
drawing, the PCB house can process the boards to meet the end-product
requirements.  If a minimum hole size is needed, in the case of a via,
the drawing should state this and not allow the hole to finish below the
minimum.  

Don't short change the PCB house - we have a fair understanding of many
of you products and more importantly how to get the there for the OEM.
Supposing the designer will understand the multitude of variables that
are inherent in PCB fabrication is much more remote than the house
having a handle on thermal and capacity management obstacles.     

Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED 
           76 Technology Drive - POB 1890 
              Brattleboro, Vermont 05302
                Voice - 802.257.4571 ext 21
                    Fax - 802.257.0011
                       <http://www.vtcircuits.com/> 
                           

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Wednesday, April 26, 2006 3:35 PM
To: [log in to unmask]
Subject: Re: [TN] Drill specification

Hi Jeff,
You say: "...the PCB house ... may opt to alter the drill size based on 
several factors -size, geometry, aspect ratio, etc."
This assumes, that the PCB house knows something about the operational
use of 
these PCBs-rarely the case, or that it knows more than the designer what
is 
needed-too often the case.
However, for knowledgeable designers that design a high-reliability
product, 
particularly for severe operational environments, and who know the 
capabilities of the PCB house, it is much better to specify the drilled
hole diameter-
again all too often not the case.

Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2