What if the "finished hole diameter after plating" is how it is worded
on the drill drawing? Can the fab house adjust the drill size dependant
on the amount of copper that will be plated into the holes? We run 2, 4
and 6 ounce boards and our fab house will drill a larger hole to plate
more copper in the hole. The logic being that if you are running 4
ounce copper and only having 1/4 or 1/2 ounce copper as a via or plated
hole won't cut the current load transfer from side to side.
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Wednesday, April 26, 2006 3:35 PM
To: [log in to unmask]
Subject: Re: [TN] Drill specification
Hi Jeff,
You say: "...the PCB house ... may opt to alter the drill size based on
several factors -size, geometry, aspect ratio, etc."
This assumes, that the PCB house knows something about the operational
use of
these PCBs-rarely the case, or that it knows more than the designer what
is
needed-too often the case.
However, for knowledgeable designers that design a high-reliability
product,
particularly for severe operational environments, and who know the
capabilities of the PCB house, it is much better to specify the drilled
hole diameter-
again all too often not the case.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|