TECHNET Archives

April 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Thu, 20 Apr 2006 14:22:10 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (AZ75)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="US-ASCII"
From:
"Whittaker, Dewey (AZ75)" <[log in to unmask]>
Parts/Attachments:
text/plain (73 lines)
I've used it and made it. Be very , very, very afraid. Do Not Use It.
Dewey 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, April 20, 2006 2:18 PM
To: [log in to unmask]
Subject: [TN] Parylene Coating Removal...

Hi All!
 
I've always thought that when it comes to removing parylene coating,
about the only way you can remove it is with some sort of mechanical
means, i.e.; microabrasion, or scraping. Burning through it with a
soldering iron when trying to do rework it is very, very
difficult...I've tried it...it doesn't work well at all.
 
I was just told that a chemical that I haven't heard of before might
work, it's called THF, or Tetrahydrofuran. I was told that it won't
dissolve the coating, but will cause it to lift from the PCB where it
can be brushed away. Have any of you ever heard of this stuff? I'm not a
chemist, and I'm not about to use it until I learn more about it.
 
The issue that I have is with a little tiny assembly that has been built
and parylene coated with some bad programmable hall effect switches
installed. The board is so small, and there are other components
installed really close to where the coating has to be removed. I'm
afraid of getting them microblasted because I'm afraid of damaging the
other components. See the assembly at:
http://stevezeva.homestead.com/files/8001_assy_backside.JPG ...the small
components are 0402's, so that gives you a visual scale of how big the
assembly is...
 
I've got the information in to a company that I found that does laser
ablation to remove coatings to give us a quote, so I'm waiting on that.
But if that turns out to be really expensive, I was contemplating using
the THF as plan "B" (provided the stuff will work and it doesn't hurt
anything else on the assembly).
 
Kind regards,
 
-Steve Gregory-
Senior Production Engineer
OAI Electronics
East 12th Street
Tulsa, Oklahoma 74112
 
(918) 836-9077 Ext.-507
(918) 706-2779 CELL

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2