I will try to test my memory here on some of the things which I glanced over
recently. Nano experts are welcome to make additions and corrections.
Nanotubes are already used in composite structures to enhance their
strength. Nanotube strength has been simulated to be very high.
Nanotubes have been used to enhance conductivity of conductive adhesives.
Separation caused by the presence of adhesives is reduced with the proper
distribution of nanotubes which provide conductive paths between the
conductive particles while staying in the adhesive.
DNA can be conductive, semiconducting or insulative depending on its
structure. This opens a vast field of research but actual devices in
manufacturing could be years away.
Metal like gold can be attached in symmetry to DNA.
Silver has been grown around DNA to create a nanowire.
Nanowires of various materials have been demonstrated (No DNA involved
here). They will aid future miniaturization progress.
DNA strands have been shown to perform complex computations by the
elimination or creation of desired and undesired combinations.
DNA can be used to make memory or computing media, may be hexabytes in a
cubic cm.
Packed nanoparticles have much higher strength than the same material in
bulk.
Thermal spray to produce nanoparticles or nanolayers of materials gives rise
to miniaturization. They also are shown to have enhanced mechanical
properties.
Future systems can be based on DNA because of its special properties.
Etc.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Selva Suganthi
Sent: Friday, April 28, 2006 7:25 AM
To: [log in to unmask]
Subject: [TN] nanotechnology
Dear All,
Pls explain me about nanotechnology ? How does it effect the semiconductor
field ?
Thanks and Regards
Suganthi,CID
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
"An ounce of action is worth a ton of theory"
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|