Most any shop can install filled via in pad technology. It is, however, a
difficult process and requires some technical expertise and equipment. If
you do not have a steady stream of this product it is difficult to both
justify the cost and maintain an efficient technology. Consequently, it has
become a specialty item.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: "Dave Seymour" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, April 19, 2006 11:17 AM
Subject: [TN] Via in Pad
> General polling question -
>
> Two of our current PCB fab vendors sub-contract out to other firms
> the application of Peters Paste for plugging vias for via in pad
> designs, and
> then bring the boards back in-house for the final plating and finishing
> the boards up.
> The above step often adds one day to current lead times.
>
> Just Curious.
>
> Why don't all fab vendors have this capability in house?
>
> Do all fab vendors sub-contract this process step out of house?
>
> Is the process so different from the normal pcb process, that Via in pad
> should be avoided?
>
> Thanks for any response.
>
> Dave
>
> --
> Dave Seymour, CID+
> Catapult Communications Inc.
> 800 Perimeter Park Dr, Suite A
> Morrisville, NC 27560
>
> Direct: (919)653-4249
> Main: (919)653-4180
> Fax: (919)653-4297
>
> [log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|