I couldn't have said it better. Bottom line, if you do have heel
overhang, you will not meet the criteria define in IPC-A-610 for minimum
heel fillet for any class of product.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US
SSA)
Sent: Monday, March 06, 2006 2:57 PM
To: [log in to unmask]
Subject: Re: [TN] Heel Overhang
There is no need to define criteria for heel fillet overhang. As Jason
notes below, the spec defines a minimum acceptable heel fillet, and if
the heel overhangs the pad, there won't be any fillet at all.
-Joe
-----Original Message-----
From: Jason Gregory [mailto:[log in to unmask]]
Sent: Monday, March 06, 2006 2:03 PM
To: [log in to unmask]
Subject: Re: [TN] Heel Overhang
Kevin,
In IPC-A-610 Rev. D, it states clearly, for Class 3, "Minimum heel
fillet
height is equal to solder thickness plus lead thickness."
If you have parts where the pad layout spread is larger than your
component,
then the larger the difference will get you further away from the
acceptable
spec.
Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)594-0602 cell
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Glidden
Sent: Monday, March 06, 2006 10:29 AM
To: [log in to unmask]
Subject: [TN] Heel Overhang
Hello again.
Question on IPC-610 (class 3) criteria. For SMT solder joints, there
appear
to be criteria set for TOE overhang, but not HEEL overhang. Is this an
oversite or a purposeful omission? Is there a limit on how much the
heel of
an "L" shaped SMT lead can be off the pad lengthwise? The obvious and
defined limit is "does not violate minimum electrical clearance", but
does
anyone else have info on this criteria?
Thanks again,
Kevin Glidden
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|