Hi Phil: They can add a "sealing" step after chromating to help prevent
fingerprinting.
Mike B.
-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
Sent: Friday, March 03, 2006 5:02 AM
To: TechNet E-Mail Forum; Barmuta, Mike
Subject: RE: [TN] "chrome" conversion of aluminum chassis
Mike,
We too are Class 3 using 5052 aluminum. In my conversations with
MacDermid, their NCP product works extremely well on 5052.
What is your solution for the fingerprints?
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Barmuta, Mike
Sent: Thursday, March 02, 2006 4:32 PM
To: [log in to unmask]
Subject: Re: [TN] "chrome" conversion of aluminum chassis
Phil: It depends on what you are using the coating for. Class 1A, Class
III, painted, unpainted, environmental exposure, type of alloy, etc.
We have looked at both MacDermid's NCP and Sanchem's Safegard CC
hexavalent chromate conversion replacements.
We are using them as an unpainted class III finish for electrical
contact NOT as a class 1A. These will be in a fairly benign environment.
We are in the process of doing electrical and environmental testing but
not salt spray/fog.
My gut feel is they may not protect as well as a class 1A hexavalent
chrome finish when scratched i.e. no self healing properties. I believe
there is also an issue with high copper aluminum alloys and salt
spray/fog resistance.
Yes, we have also seen issues with fingerprinting.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Thursday, March 02, 2006 7:47 AM
To: [log in to unmask]
Subject: [TN] "chrome" conversion of aluminum chassis
Good morning all,
As we move forward with RoHS and in an attempt to comply we are changing
the surface treatment of all our metal chassis parts.
Hexavalent Chrome Alodine or Iridite conversion processes are being
replaced with either a Trivalent Chrome Process (TCP) or Non Chrome
Process (NCP) for surface treatment of aluminum (aluminium for the Brits
out there).
What good, bad or ugly tales do you have? I know fingerprints are an
issue with some platings.
Has anyone changed processes and run salt spray tests? What were the
results?
I'm trying to put together some supporting (or refuting) data on
possible chemistries for conversion coatings to be able to defend our
change decisions.
Thanks in advance,
Phil Nutting
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
This message (including any attachments) contains confidential
and/or proprietary information intended only for the addressee.
Any unauthorized disclosure, copying, distribution or reliance on
the contents of this information is strictly prohibited and may
constitute a violation of law. If you are not the intended
recipient, please notify the sender immediately by responding to
this e-mail, and delete the message from your system. If you
have any questions about this e-mail please notify the sender
immediately.
Ce message (ainsi que les eventuelles pieces jointes) est
exclusivement adresse au destinataire et contient des
informations confidentielles. La copie, la communication ou la
distribution du contenu de ce message sans l'accord prealable de
l'expediteur sont strictement interdits et peuvent constituer un
delit. Si vous n'etes pas destinataire de ce message, merci de le
detruire et d'avertir l'expediteur. Si vous avez des questions se
rapportant a ce courrier electronique, merci de bien vouloir
notifier
l'expediteur immediatement.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
This message (including any attachments) contains confidential
and/or proprietary information intended only for the addressee.
Any unauthorized disclosure, copying, distribution or reliance on
the contents of this information is strictly prohibited and may
constitute a violation of law. If you are not the intended
recipient, please notify the sender immediately by responding to
this e-mail, and delete the message from your system. If you
have any questions about this e-mail please notify the sender
immediately.
Ce message (ainsi que les eventuelles pieces jointes) est
exclusivement adresse au destinataire et contient des
informations confidentielles. La copie, la communication ou la
distribution du contenu de ce message sans l'accord prealable de
l'expediteur sont strictement interdits et peuvent constituer un
delit. Si vous n'etes pas destinataire de ce message, merci de le
detruire et d'avertir l'expediteur. Si vous avez des questions se
rapportant a ce courrier electronique, merci de bien vouloir
notifier
l'expediteur immediatement.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|