TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stolar, Paul W" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stolar, Paul W
Date:
Thu, 2 Mar 2006 10:31:00 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (59 lines)
The temperature is the key. Most fail. Many melt. I had to give up on
this because even though I found some hi temp ones, they proved
inconsistent for range. The range decreased from about 6" to less than
1".

Paul Stolar
Materials/Reliability Engineer
Manufacturing Reliability Lead Engineer
Baker Atlas
713-625-5376
713-625-4949 (fax)


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Zarrow
Sent: Thursday, March 02, 2006 9:48 AM
To: [log in to unmask]
Subject: Re: [TN] RFID TAGs in Reflow

Mike
I suggest you contact Francois Monette at Cogiscan (_www.Cogiscan.com_
(http://www.Cogiscan.com) ).  They are masters of  RFID and material
handling,
specifically for our industry  (RFID enabled  smart feeders, MSD, etc).
RFID is the way to go, in general. Off hand, I know of RFID tags that
survive bake-out temps (per J-STD 033) but not so sure about reflow.

Phil Zarrow
ITM Consulting
Durham, NH  USA
_www.ITMconsulting.org_ (http://www.ITMconsulting.org)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2