Soldering a PTH component from pin to adjacent pin goes against standard practice for just the reasons you mention. Here's a link that is based on IPC-7711 procedures that clearly document that PTH pins should be soldered randomly to avoid heat build-up and damage:
http://www.circuittechctr.com/guides/7-2-1.shtml
-Steve Gregory-
Pradeep <[log in to unmask]> wrote:
This is Pradeep from Micropack Limited, India, fabricators of high layer count MLB's
Few of our customers are following hand soldering of multilayer PCB's for both through hole components as well as SMD's. Couple of stray cases of failure of the PTH has been reported and the analysis shows this has happened only for hand soldered boards.
Few of my queries are
1. The separation is mostly on the adjacent layer to the outer layers.
2. Why is that it is happening only for hand soldered boards
3. Somebody can help us with some reference articles on the advantages and disadvantages of both hand soldering as well as machine soldering.
4. The customer keeps telling that the soldering operator is trained and with 'years of experience' and can not make a mistake!
He keeps soldering the the pads one by one, evenif the pads are adjacent ones. We feel by doing so, the area is getting heated up to higher levels which can be avoided by soldering the pads which are not close sequentially
Rgds
Pradeep
Micropack Limited
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|