Hi Phil,
We build things for the aerospace and military market. So far we are
exempt but I'm sure that will change in the near future. In the mean
time we are stuck dealing with a dual system, component manufacturers
scrambling to supply lead free parts while we use leaded solder.
KennyB
-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
Sent: Tuesday, March 28, 2006 6:15 AM
To: [log in to unmask]
Subject: Re: [TN] Nickel Lead Finish
Ken,
Can I assume you do not send anything to Europe to Japan? If you are
assembling parts to IPC-A-610, Class 3 that does not exempt you from
RoHS.
Can't help you on the solderability info.
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bloomquist, Ken
Sent: Tuesday, March 28, 2006 9:11 AM
To: [log in to unmask]
Subject: [TN] Nickel Lead Finish
We were just notified by one of our capacitor manufacturers that they
were going lead free and their replacement finish will be nickel. These
are surface mount parts.
If my memory serves we had trouble soldering nickel leads some years ago
on some TO-5 parts.
We are a class 3 manufacturer and will continue to use lead in our
solder. Should we be concerned about the solderability of the nickel
lead finishes?
Thanks,
KennyB
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|