Thanks David.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Suraski
Sent: Tuesday, March 21, 2006 4:25 PM
To: [log in to unmask]
Subject: Re: [TN] mixing lead-free solders
Hi Phil,
The intermix between SAC305 and SN100C is fine. An article that
discusses this is available at
http://circuitsassembly.com/cms/content/view/2874/95
Best regards,
David Suraski
AIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Tuesday, March 21, 2006 4:07 PM
To: [log in to unmask]
Subject: [TN] mixing lead-free solders
Good afternoon,
As we move further into LF conversion I was curious what you, the gurus
of TechNet, thought about the possibility of mixing LF solder alloys.
We are converting our manufacturing operation to SAC 305 for wave and
hand solder. We have a CM that is using Sn100C in their wave. There is
the potential to have to manually repair a board built with Sn100C by
hand soldering with SAC 305. Are there any reliability issues with
this? Assume the board will be properly cleaned after soldering.
I haven't looked into our SMT CM and their process, but it could be
similar.
I'd hate to have to run three or four lines to keep each alloy separate.
As it is I must manage Sn/Pb and SAC 305.
Thanks in advance.
Phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|