TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Tony Gasso <[log in to unmask]>
Date:
Tue, 7 Mar 2006 16:32:19 -0500
Reply-To:
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (50 lines)
We use chart recorders and humidifiers year round to maintain RH between 40
and 50 percent. In our building, in this climate there does not seem to be a
season where we need to dehumidify.


At one of my previous employs there were occasions when we needed to
dehumidify and other seasons when we needed to humidify. Initially, we had
no control, then we installed good equipment to control temperature and
humidity.

Our insertion and placement equipment performed measurably better.

We saw a measurable improvement in first pass yields at ICT. With fewer
unexplained failures in J-FET op amps, DACs, and small signal MOSFETS.

We saw less process variation, fewer process indicators like blow holes and
pin holes, at the solder wave. We were able to extend the time between
change out of the foam fluxer.

We had fewer problems controlling performance of the vapor cleaners.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Tony Gasso
Sent: Tuesday, March 07, 2006 3:56 PM
To: [log in to unmask]
Subject: [TN] Positive Pressure


Recently a customer has requested we comply to paragraph 3.6.1 to maintain
positive presure in our facility during soldering operations, for
terminals, wire preping, limited radial components and PCBA's per J-STD-001C

We have an open assemlby area of about 10,000 Sq. Ft., lowered 12' drop
ceilings, and AC but internal doors remain open to both the fabrication
area as well as to the parking lots outside. Other than placing chart
recorders to monitor pressure, temp. and himidity, does anyone else have
similar problems with maintaining environmental controls in your facility
and have you had any positive results with your controls?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2