I previously sent Steve Gregory a picture of dendrite growing along the
glass fiber bundle from one drilled hole to the next. So- metallic paths can form
within the body of the PWB laminate, mask, via to via, etc., if you give
them half a chance to generate internal shorts.
[Steve- you might want to re-post that picture if it is no longer on your
site (if there are TNetters who would like to have it.)]
Bill Kenyon
Global Centre Consulting
3336 Birmingham Drive
Fort Collins, CO 80526
Tel: 970.207.9586 Cell: 970.980.6373
email: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------