Joe,
Thanks.
I hope there will be more comments particularly from producers and users of
punched PWBs. Coming from the mainstream, punching seems to be a lost art.
I am concerned about punching multilayers particularly with the newer
materials that we use today which might not have been evaluated or
formulated for punching.
Thanks,
Gerry
From: Joe Fjelstad <[log in to unmask]>
Reply-To: TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
To: [log in to unmask]
Subject: Re: [TN] Die Punching PWBs as opposed to drilling and NC routing
Date: Fri, 17 Mar 2006 16:00:16 EST
NC drills are highly versatile and stacking panels provides some economy
and
so it will be hard to displace them.
Punching can be fast (all holes at once) but is one at a time and depending
on approach, hole count and feature size the tooling might be costly and
must
be amortized over a number of panels to pay for the tool.
Hole quality is not as good making plating more of a challenge if you plan
on doing double sided PCBs. I have not heard of MLBs being punched (except
when the drills got too dull ;-)
There should also be some concerned about punching small holes on fine
pitch
in glass fabric as there would be a higher risk of CAF, however for polymer
films it is not so much of an issue.
I expect there will be other comments coming.
Joe
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
_________________________________________________________________
Don’t just search. Find. Check out the new MSN Search!
http://search.msn.click-url.com/go/onm00200636ave/direct/01/
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|