The attraction to me is that real data overcame the potential residual
effects elsewhere.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Wednesday, March 08, 2006 6:15 AM
To: [log in to unmask]
Subject: Re: [TN] soldering to PdAg cap
Hi Guy! The use of Sn62 will slow down the leaching of the terminal but
you are still going to lose PdAg thickness. And you should be cautious
on any secondary soldering operations because you have the possibility
of completely leaching off the PdAg termination if you hand solder it a
second time (I have seen components fall off pwas). Does your customer
have real data demonstrating that a nickel or copper barrier layer on
the capacitors will cause a functional issue? The reason I ask is I once
worked with a program where the electrical engineers swore that the
nickel barrier was going to be a huge functional issue. When they
started having capacitors fall off the pwas (our soldering options were
such that I couldn't prevent/minimize the leaching actions) the
equivalent capacitor with a nickel barrier was used with no functional
impact. Funny how real data matters! Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Guy Ramsey
<gramsey@RDCIRCUI
TS.COM>
To
Sent by: TechNet [log in to unmask]
<[log in to unmask]>
cc
Subject
03/07/2006 01:35 [TN] soldering to PdAg cap
PM
Please respond to
gramsey@rdcircuit
s.com
We are leaching the termination off of a capacitor. Our customer
requires a non-magnetic component and has specified a component without
a nickel barrier, because of nickel's ferromagnetic properties.
What can we do?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|