TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Kane, Amol (349)" <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 3 Mar 2006 07:40:16 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Stephen Gregory <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Stephen Gregory <[log in to unmask]>
Parts/Attachments:
text/plain (115 lines)
Hi Amol!

It was 63/37 solder...only the board was finished with ImAg...

-Steve Gregory-

-----Original Message-----
From: Kane, Amol (349) [mailto:[log in to unmask]] 
Sent: Friday, March 03, 2006 6:15 AM
To: TechNet E-Mail Forum; Stephen Gregory
Subject: RE: [TN] As long as we're talking about silver...

What solder did you use for the wave?? We did our first lead-free run
not too long ago.

Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing 
941 Route 38  Owego, NY 13827
Phone: (607) 687-7669 x349
[log in to unmask]

 -----Original Message-----
From:   TechNet [mailto:[log in to unmask]]  On Behalf Of Stephen Gregory
Sent:   Thursday, March 02, 2006 5:15 PM
To:     [log in to unmask]
Subject:        [TN] As long as we're talking about silver...

Hi All!

 

I figured as long as we're talking about silver, you might take a look
at some PTH solder joints on some boards we just built with an immersion
silver finish. I'm posting these pictures because this is the first
production board we've built here that has an ImAg finish, and I would
like to know if this appearance is pretty typical. Go check out:

 

http://stevezeva.homestead.com/files/Immersion_Silver_PTH.jpg

 

http://stevezeva.homestead.com/files/Immersion_Silver_PTH_2.jpg

 

This particular board went through double-sided reflow, and then the PTH
was soldered using a selective wave solder pallet while being fluxed
with an ultrasonic spray fluxer using Kester 2331ZX OA flux.

 

You can see that the solder didn't flow out to the edges of the pads on
the primary side of the board, the secondary side of the board looks
wonderful.  I know this is not a defect according to the -610...but is
this typical? Especially since it went through two reflow cycles?

 

Thanks in advance!

 

-Steve Gregory-

 

 



_______________________________________________________
This message may contain information that is privileged and confidential
to LaBarge, Inc. It is for use only by the individual or entity named
above. If you are not the intended recipient, you may not copy, use or
deliver this message to anyone. In such event, you should destroy the
message and kindly notify the sender by reply e-mail.


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------




_______________________________________________________
This message may contain information that is privileged and confidential to LaBarge, Inc. It is for use only by the individual or entity named above. If you are not the intended recipient, you may not copy, use or deliver this message to anyone. In such event, you should destroy the message and kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2