You nailed it Richard! If it was wave soldered then it would be an easy
problem but hand soldering is not that controlled.
I think some of the suggestions for achieving a good solder joint will
go a long way toward making good solder joints but the inspection
problem still remains.
I'm going to look into adding a washer to raise the connectors up a tad
but due to tolerance build up this may not be possible.
KennyB
-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: Wednesday, March 01, 2006 6:30 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Joint Inspection
This is a good suggestion. You can use a few scrap boards or solder
coupons.
The trouble is that you cannot really control the process well enough to
know you are getting consistant results because of the fact that they
are hand-soldered, and the operator/equipment/methods variability will
eventually cause a worst-case scenario. If the boards were wave-soldered
under controlled methods it could be done.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|