TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 31 Mar 2006 13:56:41 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
John Burke <[log in to unmask]>
Parts/Attachments:
text/plain (184 lines)
If you want the book you can get it on ebay..............8-)

You can get anything on ebay.....here is the link

http://tinyurl.com/f2t7v


John Burke
Senior Manager - Operations , Optichron
[log in to unmask]
W: 510 249 5233
M: 408 515 4992
http://www.optichron.com
Profile: https://www.linkedin.com/e/fps/2665502/

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Friday, March 31, 2006 1:07 PM
To: [log in to unmask]
Subject: Re: [TN] IPC Surface Analysis Synopsis?

There is an excellent summary detail of failure analysis methods at
semicon fareast website. Check it out at
http://www.semiconfareast.com/fa.html. Click on FA methods, they have
good descriptions of them all. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Schaefer, Chris
Sent: Friday, March 31, 2006 12:36 PM
To: [log in to unmask]
Subject: Re: [TN] IPC Surface Analysis Synopsis?

Hey Dave,

Where can we get a copy?

Chris Schaefer
Suntron Corporation
Process Engineer
540 N. Rogers Road
Olathe, Kansas 66062
913.393.5878
[log in to unmask] 

NOTICE:
 
This message is intended for the use of the individual entity to which
it is addressed and may contain information that is privileged,
confidential and exempt from disclosure under applicable law. If the
reader of this message is not the intended recipient, or the employee or
agent responsible for delivering the message to the intended recipient,
you are hereby notified that any dissemination, distribution or copying
of this communication is strictly prohibited. If you have received this
communication in error, please notify us immediately by calling
913.393.5878 or returning the original message to us.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of David D. Hillman
Sent: Friday, March 31, 2006 12:31 PM
To: [log in to unmask]
Subject: Re: [TN] IPC Surface Analysis Synopsis?


Hi Rich! I don't know of any IPC document but I do have a really good
technical reference that my be of use:

Ewing's Analytical Instrumentation Handbook, edited by Jack Cazes, ISBN
0-8247-5348-8

This book covers everything: FTIR, IC, SEM, Xray, GC, HPLC, DSC, TGA,,
AA, ICP, etc.

Dave



             Richard
             Kraszewski
             <[log in to unmask]
To
             COM>                      [log in to unmask]
             Sent by: TechNet
cc
             <[log in to unmask]>
 
Subject
                                       [TN] IPC Surface Analysis
Synopsis?
             03/31/2006 07:33
             AM


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
                  Richard
                Kraszewski
             <[log in to unmask]
                   COM>






I remember seeing a synopsis of surface analysis methods (EDX, Auger,
etc.) in some IPC standard or handbook.

Does anyone recall which document that may be?

Rich - KEDS


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2