Hi Dacia:
The solder spheres may start oxidizing when the flux stops
shielding it from the ambient. We are very strict with solder. It has a
shelf life when refrigerated, a time after it is thawed out, and a time
after it is dispensed. It is not worthy to risk to have voids in the
solder or other anomalies. Perhaps in the case of large quantities of
solder that has extended its shelf life, the best way to handle it is to
return it to the manufacturer for credit.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dacia Schoolfield
Sent: Thursday, March 23, 2006 12:15 PM
To: [log in to unmask]
Subject: [TN] Solder Paste Question
Gurus of the manufacturing industry -
What is your take on adding RMA flux to solder paste - either new paste
or used paste? Is there a difference in results when adding flux to
leaded versus non-leaded paste?
For those of you who do add additional flux to paste, what types of
controls do you have in place to ensure the paste itself is still
viable?
I understand this is an extremely general question, and am looking for
general answers.... or, if anyone has recommendations as far as
research, I would gladly accept all input.
I appreciate your thoughts.
Dacia
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|