Hi Mark: First of all it doesn't make sense why the customer wants to
use a leadfree solder on a leaded (C360 brass) component. It won't be
RoHS compliant. What is there reason for asking for leadfree solder?
However if ours is not to question why then give them what they are
asking for; leadfree solder.
You may have oxidized parts and need a stronger flux/deoxidizer. As a
test try dipping a few in 5% sulfuric acid for 20-30 seconds at room
temp, rinse well with cold water and dry immediately.
See if they wet better. If they do then use the acid predip or a
stronger fluxing agent. If they don't you could always tin plate them
along with a copper or nickel barrier plate and solder to the tin.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mark Clark
Sent: Tuesday, March 21, 2006 6:52 AM
To: [log in to unmask]
Subject: [TN] PB-Free Solder and Brass
I have a customer that is required to use a Lead Free solder to attach
some
brass components (battery contacts) to a PCB. What he is experiencing
is
the brass will not tin using this solder. Anyone have any suggestions:
Solder required for use:
Cookson Electronics - Alpha Cleanline 7000
Alloy 96.5Sn 3.0Ag 0.5Cu
Flux: P2
The contact material is:
360Brass
His customer is in a rush for these components, and is demanding the
Pb-free
be used.
BTW - the good old fashion No-clean and Rosin (both of these have lead
in
them) work great.
TIA
Mark Clark
Avalon Engineering, LLC
2179 Fourth Street, Suite 2D
PO Box 10789
White Bear Lake, MN 55110-0789
Phone: 651-426-8599 x202
Fax: 651-426-4418
mailto:[log in to unmask]
www.avalon-us.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
This message (including any attachments) contains confidential
and/or proprietary information intended only for the addressee.
Any unauthorized disclosure, copying, distribution or reliance on
the contents of this information is strictly prohibited and may
constitute a violation of law. If you are not the intended
recipient, please notify the sender immediately by responding to
this e-mail, and delete the message from your system. If you
have any questions about this e-mail please notify the sender
immediately.
Ce message (ainsi que les eventuelles pieces jointes) est
exclusivement adresse au destinataire et contient des
informations confidentielles. La copie, la communication ou la
distribution du contenu de ce message sans l'accord prealable de
l'expediteur sont strictement interdits et peuvent constituer un
delit. Si vous n'etes pas destinataire de ce message, merci de le
detruire et d'avertir l'expediteur. Si vous avez des questions se
rapportant a ce courrier electronique, merci de bien vouloir
notifier
l'expediteur immediatement.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|