I have a customer that is required to use a Lead Free solder to attach some
brass components (battery contacts) to a PCB. What he is experiencing is
the brass will not tin using this solder. Anyone have any suggestions:
Solder required for use:
Cookson Electronics - Alpha Cleanline 7000
Alloy 96.5Sn 3.0Ag 0.5Cu
Flux: P2
The contact material is:
360Brass
His customer is in a rush for these components, and is demanding the Pb-free
be used.
BTW - the good old fashion No-clean and Rosin (both of these have lead in
them) work great.
TIA
Mark Clark
Avalon Engineering, LLC
2179 Fourth Street, Suite 2D
PO Box 10789
White Bear Lake, MN 55110-0789
Phone: 651-426-8599 x202
Fax: 651-426-4418
mailto:[log in to unmask]
www.avalon-us.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|