Hi Jim
Since then this product has changed it's name (& manufacturer) several
times, starting with "Norplex Oak" following
with "Allied Signal" & so on to "Isola".
Right now it's available from Isola-laminate systems as A-11 No-Flow
prepreg, You can find the full description in their web site.
Regards
Shabtay
Eltek -LTD
> -----Original Message-----
> From: Marsico, James [SMTP:[log in to unmask]]
> Sent: ב 20 מרץ 2006 15:06
> To: [log in to unmask]
> Subject: [TN] No Flow Prepreg
>
> Good day, Technet:
>
> Even though I can't seem to receive e-mail from [log in to unmask]
> <mailto:[log in to unmask]> , I do receive answers to posts when they're sent
> back to me directly. So, here is a question.
>
>
>
> I have to build an old design (1980's) where we have to bond a heat sink
> to
> a PWB using a no-flow prepreg manufactured by Fortin Laminating
> Corporation,
> P/N A-11-108-65. I can't seem to find any information on Fortin
> Laminating.
> Does anyone know what happened to hem?
>
>
>
> (Please respond to ALL, so I get a copy sent to me directly.)
>
>
>
> Thanks,
>
>
>
> Jim Marsico
>
> EDO Corporation
>
> Amityville: 631-630-5079
>
> Bohemia: 631-218-7057
>
> [log in to unmask]
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|