G = E-Glass, woven,
F = Epoxy, flame resistant
N = natural color of resin system
See MIL-S-13949
Mike Green
Production Design Engineering
Lockheed Martin Space Systems
Sunnyvale, CA 94089
office 408-743-1635
Synergy works at LMC. "Show me the data."
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Steve Hodge
Sent: Tuesday, March 14, 2006 8:03 AM
To: [log in to unmask]
Subject: Re: [TN] <List>[TN] TYPE GFN Laminate
I believe it stands for "glass filled -natural (color)
At 09:10 AM 03/14/2006, you wrote:
>Hello Oracles, etc...
>
>Within our standard note for specifying bareboard material is a
reference
>to "TYPE GFN". Anyone out there know what that means? I sure don't...
>
>A quick googling finds other folks out there referencing it (along with
>definitions like 'Good For Nothing' and "Gone For Now'), but I couldn't
>locate an explanation of it's meaning related to FR4...
>
>Thanks and Happy Tuesday,
>-Chris
>
>
>"This e-mail message is intended only for the use of the intended
>recipient(s).
>The information contained therein may be confidential or privileged,
and
>its disclosure or reproduction is strictly prohibited.
>If you are not the intended recipient, please return it immediately to
its
>sender at the above address and destroy it."
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text
in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|