TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 8 Mar 2006 14:49:28 -0500
Reply-To:
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (22 lines)
Dear SIR,
could you kindly provide the update info regarding the maximum bias for the
conformal coating SIR test?  Is it still 333 V/mm?  assume I use read out at
100 Vdc and bias at 50 Vdc for the B-25A, am I right that bias max is
333V/mm and read out is at 666V/mm spacing?  Thank you very much.
Best regards,
                       jk
ps.  I know Concoat recommend low voltage bias, but the current test method
650-2.6.3.4 is still high voltage.  (50Vdc bias)... by the way, anyone has
table regarding the dielectric withstanding voltage per IPC-CC-830?  Many
thanks.)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2