Specification is 2 microinches minimum at -4sigma from the process mean,
typical values 3-5 microinches for Au, 120 to 240 microinches for Ni.
Regards
Gerard O'Brien.
Co-chair 4-14 plating committe
-----Original Message-----
From: Jones, Evamaria [mailto:[log in to unmask]]
Sent: Wednesday, March 08, 2006 10:56 AM
To: [log in to unmask]
Subject: [TN] Minimum thickness required for gold immersion finish on PTH
and Vias
Question,
Does anyone out there know the minimum thickness required for a gold
immersion finish for PTH's and Vias. A colleague ask me and I don't have a
copy of the IPC-4552. There was an article in Printed Circuit Design and
Manufacture in February 2006 titled Know Your Surface Finish. It recommended
2-4 uin". I admit...I am an assembly gal not a PWB fab gal. What does the
spec say? The article was not very favorable toward Imm. AG. Any warnings or
risks?
Evamaria
Quality Engineer
Instructor
________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|