Subject:
From:
Lee parker <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Lee parker <[log in to unmask]>
Date:
Thu, 23 Feb 2006 08:29:16 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (86 lines)
As Scott said, these two finishes are different. By t
Selva



As Scott said, these two finishes are different. By the way the term normally used is Flash Gold. Flash Gold uses electrolytically plated soft gold over electrolytically plated nickel and thus enjoys several advantages over ENIG. 



I coauthored a paper at EXPO on this finish. I have worked with several clients who have migrated from ENIG to Flash Gold and have found it to be a great success Oddly enough, the finish is for the most part supplied by PCB shops in China and Taiwan.



Best regards



Lee



J. Lee Parker, Ph.D.

JLP Consultants LLC

804 779 3389 

  ----- Original Message ----- 

  From: Scott B. Westheimer<mailto:[log in to unmask]> 

  To: [log in to unmask]<mailto:[log in to unmask]> 

  Sent: Thursday, February 23, 2006 7:51 AM

  Subject: Re: [TN] Question regd surface finish.





  Selva.



  They are not the same. ENIG is electroless nickel under immersion gold which

  is 3 to 5 micron thick and it a soft gold finish. Gold flash in applied also

  over nickel and is electro plated. The thickness can be made thicker than

  immersion gold by increasing the time in the tank. Electro plated gold can

  be either hard or soft.



  Scott B. Westheimer

  ----- Original Message -----

  From: "Selva Suganthi" <[log in to unmask]<mailto:[log in to unmask]>>

  To: <[log in to unmask]<mailto:[log in to unmask]>>

  Sent: Thursday, February 23, 2006 5:38 AM

  Subject: [TN] Question regd surface finish.





  > Dear All,

  >

  > I have a query regarding surface finish,

  >

  > I saw one fabinstruction notes  , there the surface finish mentioned as

  > Gold flash , my query is "Are  the term Gold finish and ENIG both  mean

  > same ? or do they different ?" if so let me know the difference.

  >

  > Thanks in advance!!

  >

  > Thanks and Regards

  > Suganthi

  >

  > ---------------------------------------------------

  > Technet Mail List provided as a service by IPC using LISTSERV 1.8e

  > To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in

  > the BODY (NOT the subject field): SIGNOFF Technet

  > To temporarily halt or (re-start) delivery of Technet send e-mail to

  > [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)

  > To receive ONE mailing per day of all the posts: send e-mail to

  > [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest

  > Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>

  > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>

  > for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or

  > 847-615-7100 ext.2815

  > -----------------------------------------------------

  > "Progress is the activity of today and the assurance of tomorrow."

  >



  ---------------------------------------------------

  Technet Mail List provided as a service by IPC using LISTSERV 1.8e

  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in

  the BODY (NOT the subject field): SIGNOFF Technet

  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)

  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest

  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>

  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815

  -----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2