I have this, but I seem to be missing some chart info.
Ken
Coefficient, X 10-5
Material Lenghtwise Crosswise
FR-2 1.2 2.5
FR-3 1.3 2.5
FR-4 1 1.5
FR-5 1 1.5
FR-6 1 1
CEM1 1.1 1.7
CEM3 1 1.5
G-10 1 1.5
G-11 1 1.5
GI 1 1.2
GT 1 2.5
GX 1 2.5
Polystyrene 7 7
Cross-linked polystyrene 5.7 5.7
--------------------------------------------
Kenneth J. Wood C.I.D.
Saturn PCB Design
www.saturnpcb.com
407-340-2668
----- Original Message -----
From: "Gregg A. Owens" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, February 14, 2006 5:46 PM
Subject: [TN] Coeffecient of Thermal Expansion (CTE) Rates
> Dear Technetters:
>
>
>
> Anyone have a source for different CTE rates for common elements used in
> electronic assemblies?
>
>
>
> Any input appreciated.
>
>
>
> Gregg A. Owens
>
> Master IPC Instructor
>
> Executive Director
>
> Manufacturing Technology Training Center, Inc.
>
> 10427 San Sevaine Way, Suite 'I"
>
> Mira Loma, CA 91752 USA
>
> Tel (951) 360-1324 Fax (951) 360-1346
>
> www.mttc-inc.com
>
>
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|