Wee Mei:
There is another approach at applying adhesive to the
package instead of to the leads. Make a bead that runs on the board up
the corner of the package and over the top of the package, repeated four
times ( one on each corner).
As far as the heel fillet it has to be up half the curve of the
heel per J-Std-001 9.2.6.1. The customer may buy the strengthening of
the package to the board bond by adding the adhesive, specially if it
passes all tests.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wee Mei
Sent: Monday, February 06, 2006 6:24 PM
To: [log in to unmask]
Subject: Re: [TN] Gull wing side & toe fillet height
Hello,
Since the discussion is about gull wing package, I would like to ask one
question : "Is there a minimum requirement for heel fillet"? The reason
I asked is that we encounter soldermask inside the via-in-pad for solder
pads.
As a result, the heel of the gull wing package happen to rest over this
via-in-pad that has soldermask inside. Being a TQFP64 package and pad
width of 16mil with the via diameter as 12mil, there is hardly any room
to provide solderability to the back of the lead heel. If you can image,
there isn't or very little possibility of solder fillet that can be
formed at the heel.
For me I would consider this as failure. However, the board is urgently
require and would be ESS, can enhancing the soldered leads reliability
by applying adhesive over them help?
Looking forward to your reply,
Thanks,
Wee Mei
----- Original Message -----
From: "Rex Waygood" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, February 07, 2006 1:03 AM
Subject: Re: [TN] Gull wing side & toe fillet height
> IPC 610 Rev D ( 8.2.5.4???) Side Fillet is by length and evidence of
> wetting, no height.
> The reason you cannot find a toe requirement is that there is not one.
> Components often have a pre-plated cropped end so it isn't necessarily
> wettable. You are also allowed toe overhang of the pad.
> Rex
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of sumxp
> Sent: 06 February 2006 15:23
> To: [log in to unmask]
> Subject: Re: [TN] Gull wing side & toe fillet height
>
> Sorry,I am referring to side and toe fillet Height.
>
> Thanks
>
> sumxp
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ______________________________________________________________________
> __ This email has been scanned for all viruses by the MessageLabs
> SkyScan service.
> ______________________________________________________________________
> __
>
>
>
> This email has been scanned for all known viruses by the MessageLabs
> SkyScan service.
> ================================================================
> This email (including any attachments) is confidential and/or may be
> legally privileged. It is intended for the named recipient (s) only
> and may not be forwarded, disclosed or otherwise disseminated
>
> Although this email has been scanned for viruses, WE DO NOT (to the
> extent permitted by law) ACCEPT ANY LIABILITY WHATSOEVER for any virus
> infection, compromise of security or losses resulting from vi
>
> NO CONTRACT MAY BE FORMED OR DOCUMENTS SERVED BY THIS EMAIL unless
> specifically agreed to in writing and signed by a Director of
Hansatech.
> Any views or opinions expressed in this email are those of
>
> If you have received this email in error please contact the IT
> department immediately on (01202) 674 333 or (01553) 691 022 prior to
deletion.
> ================================================================
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|