I thank all of you who provided this information on IS410 and Polyclad
370 HR, and also to the person who provided information on the handheld
scanner for identifying RoHS contaminants.
There is so much valuable information on Technet.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Friday, February 24, 2006 10:55 AM
To: [log in to unmask]
Subject: Re: [TN] IS410 FR-4 laminate
Typo,
160 should of course read 260
John
John Burke
Senior Manager - Operations , Optichron
[log in to unmask]
W: 510 249 5233
M: 408 515 4992
http://www.optichron.com
Profile: https://www.linkedin.com/e/fps/2665502/
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Friday, February 24, 2006 8:52 AM
To: [log in to unmask]
Subject: Re: [TN] IS410 FR-4 laminate
POlyclad 370 HR is just amazing, never did manage to break it with
thermal cycling to 160 degrees. We did it 15 times to 260 to the Jedec
020C profile, and it tested just fine after each cycle on ICT, and no
delamination.
John
John Burke
Senior Manager - Operations , Optichron
[log in to unmask]
W: 510 249 5233
M: 408 515 4992
http://www.optichron.com
Profile: https://www.linkedin.com/e/fps/2665502/
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(AZ75)
Sent: Friday, February 24, 2006 5:51 AM
To: [log in to unmask]
Subject: Re: [TN] IS410 FR-4 laminate
That's like switching from a Toy Poodle to a King Charles Spaniel. A
definite improvement and with the right handler can perform well. Now if
you want to play in the Lead-Free Arena with all around performance in
any field, step up to the Working Dog Group.
Polyclad 370 HR and MEM 1755 are the current ribbon contenders.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Scott Lefebvre
Sent: Thursday, February 23, 2006 5:46 PM
To: [log in to unmask]
Subject: [TN] IS410 FR-4 laminate
I am looking to switch from Nelco N4000-6 to Isola IS410 laminate. I
wanted to know if anyone would be willing to share there experience with
this material. This material will be used in a lead free process.
Any advice would be greatly appreciated thanks in advance.
Scott Lefebvre
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|