TECHNET Archives

February 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Dwight Mattix <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 2 Feb 2006 16:16:04 -0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Marcello Brett Malteze <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Marcello Brett Malteze <[log in to unmask]>
Parts/Attachments:
text/plain (155 lines)
Hi Mattix,
 
    I  always called him Mr. Hoover since he worked for us at Multekl!!! Do
you have your new email because hi is not more at Multek group until I
know!!!
 

Marcello Brett Malteze 
Mechanical Process Engineering 
Multek Brazil 
Phone: + 55 11 3749 8384 
Mobile: + 55 11 9468 4833 
Skype: mbrett73 
Email: [log in to unmask] 

 

  _____  

From: Dwight Mattix [mailto:[log in to unmask]] 
Sent: quinta-feira, 2 de fevereiro de 2006 16:08
To: TechNet E-Mail Forum; Marcello Brett Malteze; [log in to unmask]
Subject: Re: [TN] Via on Hole process


MR.(?) Hoover!!!

That's makes him sound sooo respectable.  He's still just "Groovy" to most
of us.

dw


At 10:00 AM 2/2/2006, Marcello Brett Malteze wrote:


Hi Jeffrey,

        Tks a lot for you feedback and do you have the papers from Mr.
Hoover?Would you send to me?

Tks a lot


Marcello Brett Malteze
Mechanical Process Engineering
Multek Brazil
Phone: + 55 11 3749 8384
Mobile: + 55 11 9468 4833
Skype: mbrett73
Email: [log in to unmask]


-----Original Message-----
From: Jeffrey Bush [mailto:[log in to unmask]
<mailto:[log in to unmask]> ] 
Sent: quinta-feira, 2 de fevereiro de 2006 11:32
To: TechNet E-Mail Forum; Marcello Brett Malteze
Subject: RE: [TN] Via on Hole process

Buried vias should not need to be filled as the bonding material should
adequate to fill these features to minimum standard.  

If you as discussing the filling of thru-hole vias, I would recommend a
Peters SD2795 and the investment in a planarization unit.  Traditional
scubbing is problematic and we have attempted using the Ishii Hyoki
mechanical as well as a chemcut unit.  The best process we have determined
is using a Pola&Massa process to remove the surface epoxy as well as reduce
the surface copper improved by the plating of the via prior to filling.
Your Dave Hoover presented a great paper at SMTA/Dallas in 2004, where the
various processes are discussed for via filling.       

Jeffrey Bush
Director, Quality Assurance and Technical Support VERMONT CIRCUITS
INCORPORATED 
           76 Technology Drive - POB 1890 
              Brattleboro, Vermont 05302
                Voice - 802.257.4571 ext 37 
                    Fax - 802.257.0011
                       <http://www.vtcircuits.com/
<http://www.vtcircuits.com/> > 
                           

-----Original Message-----
From: TechNet [mailto:[log in to unmask] <mailto:[log in to unmask]> ] On Behalf
Of Marcello Brett Malteze
Sent: Thursday, February 02, 2006 6:17 AM
To: [log in to unmask]
Subject: [TN] Via on Hole process

Hello all,

We are installing the via on hole process and iīm looking for more
informationīs regarding to Ink Supplier to fill the buried vias , someone
that could describe the flow process and if it is possible to run
planarization on a normal Scrubex machine not Ishiihyki.

Tks a lot,

Brett

 

Marcello Brett Malteze
Mechanical Process Engineering
Multek Brazil
Phone: + 55 11 3749 8384
Mobile: + 55 11 9468 4833
Skype: mbrett73
Email: [log in to unmask] 

 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives
<http://listserv.ipc.org/archives>  Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>  for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
<http://listserv.ipc.org/archives> 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>  for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
----------------------------------------------------- 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2