TECHNET Archives

February 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Amol (349)" <[log in to unmask]>
Date:
Thu, 16 Feb 2006 09:33:06 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Phil Nutting <[log in to unmask]>
Parts/Attachments:
text/plain (136 lines)
Hey, it is vented out of the room.  Doesn't that count as zero
emissions?  OK, so there are a bunch of expired birds on the roof and
the neighbors all have nasty diseases, but it passes in-house testing.

Just kidding.

A true Zero emissions booth I would expect to have some form of scrubber
on the exhaust so the only emissions were pure air.

Phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349)
Sent: Thursday, February 16, 2006 9:12 AM
To: [log in to unmask]
Subject: [TN] Zero Emissions Spray Booth

Dear TechNetters,
A question was recently asked by a customer whether we have a "Zero
Emissions Spray Booth" for conformal coating applications. We spray
polyurethane, acrylic, epoxy and silicon coatings. We have an exhaust
type spray booth to remove harmful vapors from the coating room. Can
anyone shed some light on the Zero Emissions Spray Booth concept so that
I can evaluate our existing infrastructure against the requirements and
make upgrades if necessary.

Thanks in advance,

Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing 
941 Route 38  Owego, NY 13827
Phone: (607) 687-7669 x349
[log in to unmask]

 -----Original Message-----
From:   TechNet [mailto:[log in to unmask]]  On Behalf Of Dehoyos, Ramon
Sent:   Thursday, February 16, 2006 8:33 AM
To:     [log in to unmask]
Subject:        Re: [TN] BGA Reflow profile - Thermocouples

        Hi Dominic:
        It should not cost you much to find out what is the temperature
of a board through reflow. The investment of buying a Mole or other
similar device, that will allow you to record the profile of a board
through an oven is only "once". If you are using eutectic solder and
your coldest components sees 20 degrees over the melting point which is
203 C  and you are not exceeding the highest temp that the most
sensitive component may withstand, then you have a working profile, that
simple.
        Regards,
        Ramon

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dominic Boudreau
Sent: Wednesday, February 15, 2006 5:50 PM
To: [log in to unmask]
Subject: [TN] BGA Reflow profile - Thermocouples

Hello Techneter's,

I am working on a procedure to make the reflow profile of a PCB.

What are the techniques to know where to attach the thermocouples on the
"PCB"? I already know that it should be where we have the coldest and
hottest spot but is it possible to know when we "must" test a BGA to
have a better reflow profile. We are a little company so we don't have
the money to test a BGA each time we have one on a PCB.   

 

Thank you

 

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2