Unclear how fast you need this to set up... but, have you considered silicones?
Might be very nice alternate, because of heat resistance, and flexibility.
Rudy Sedlak
John Foster <[log in to unmask]> wrote: Hello I am looking for some adhesives.
I need to bond some fr4 circuit cards to a piece of aluminum.
The boards are extremely small and only need to survive shock
in other words not pop off from a sudden jolt.
The boards also have wires soldered to surface mount pads 15 x 30 mils
I am using 32 AWG stranded wire and was hoping to find some kind
of epoxy to put over the soldered wires to give them strength.
The boards are about the size of my thumbnail. This
has been a real challenge for my fabricator and assembler first to route the
boards out and second
to solder the 2 ICS.
Any input on the epoxy and adhesive will really be appreciated
Thank You
John Foster
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
Yahoo! Photos
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Ring in the New Year with Photo Calendars. Add photos, events, holidays, whatever.
|
|
|