TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jeffrey Bush <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Date:
Wed, 18 Jan 2006 16:39:32 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (115 lines)
I agree.

Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED 
           76 Technology Drive - POB 1890 
              Brattleboro, Vermont 05302
                Voice - 802.257.4571 ext 37 
                    Fax - 802.257.0011
                       <http://www.vtcircuits.com/> 
                           

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Wednesday, January 18, 2006 12:55 PM
To: [log in to unmask]
Subject: Re: [TN] RoHS board finish

Polyclad 370HR finished in immersion silver will be pretty much bullet
proof.

Kind regards,

John Burke

John

John Burke
Senior Manager - Operations , Optichron
[log in to unmask]
W: 510 249 5233
M: 408 515 4992
http://www.optichron.com
Profile: https://www.linkedin.com/e/fps/2665502/

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Walker
Sent: Wednesday, January 18, 2006 9:39 AM
To: [log in to unmask]
Subject: [TN] RoHS board finish

Hi All,

I'm doing my first PCB design that will use lead-free components and I
need
to change my board finish from what I've always used.....HASL. I'm
looking for
 any recommendations or comments on the best board finish to use.

The components used on the design will be a mixture of tin-lead and
lead-free (SAC), so I'm not sure if there is a preferred finish to use
in this  type
of situation. I work in a prototype environment where the boards may be
reworked (BGA removal/replaced) a number of times, so I'm concerned
about the
ability of the finish being able to handle being  reworked/reflowed a
number of
times.

I'd also welcome any recommendations on the type of board material to
use
since it will see an elevated temperature of up to 260C. I've always
just
specified FR4 in the past.

Thanx in advance for any feedback.

Regards,
Bob Walker
[log in to unmask] (mailto:[log in to unmask])

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2