Phil:
It is actually possible for a soldermask to be a bit of all those classes, however, most LPI soldermasks are predominantly acrylics. This is what makes them strippable.
Rudy Sedlak
"Crepeau, Phil (Space Technology)" <[log in to unmask]> wrote:
hi,
i'd like to know the class(es) of organic compounds that lpi soldermasks
fall into. would/could they classified as urethane, acrylic, epoxy, or
other? we need to identify the class(es) to our customer and i haven't
had much luck. i'm sure it depends on the vendor, so if i get reponses
that indicate they could fall into several classes, i'd like to know
what they all are.
thanks,
phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
Do you Yahoo!?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
With a free 1 GB, there's more in store with Yahoo! Mail.
|
|
|