TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Joel Mearig <[log in to unmask]>
Date:
Thu, 19 Jan 2006 10:50:05 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<200601181342828.SM01596@cpujoel0224>
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (61 lines)
As a general rule, water-soluble flux residues are very dangerous. They
are usually very acid and can attack metals on the assembly. At the best
they will make the solder joints matt. At the worst, increasing quantity
of the residues will form adsorption bonds with the substrate and
components within the residues may polymerise, making it
quasi-impossible to clean the residues after, say, an hour or so. It
therefore is **very** necessary that cleaning be started within minutes
of soldering. However, there is an excellent work-around that has been
proven and that can extend the hold time before cleaning to a few hours,
the use of a chelating neutraliser. Many flux manufacturers offer these
under trade names such as Neutralizer 2051, Rinse-Aid and so on. They
are mildly alkaline, buffered, room-temperature, dilute baths (pH
typically 8.5 to 9), which must NOT be confused with saponifiers, which
are unsuitable for this job. They serve many functions, but the
assemblies can stay therein, immediately after soldering/reflow, from 2
minutes up to, say, 4+ hours. They will actually improve the cleaning
quality at almost no cost. The assemblies should be cleaned within
minutes of their removal from the holding tank. The makers usually
recommend a 5% solution of the concentrate, but a 2% solution has been
proved equally effective.

You can see this technique being used on the old video at
http://www.protonique.com/video/ in the context of wave soldering.

Brian

Joel Mearig wrote:
> I am currently using a water-soluble, lead-free solder paste from Kester. I
> am trying to minimize the cleaning cycles so I leave flux on the product for
> an extended period of time. Do any of you have any recommendations on the
> amount of time flux can be left on the product without affecting the
> cleaning process? Thanks in advance for your input.
>
>
>
> Joel Mearig
>
> Delta Tau Data Systems, Inc.
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2