Hi Mike! Absolutely! I have a designer who is connecting two pwbs with one
connector. The connector "tails" protrude thru the pwbs to the outer
surfaces (basically a pwb/connector/pwb sandwich). These tails need to
remain free of solder but experience has proven that I'll get solder
wicking on the tails unless I "block" the solder flow. As Bev suggested, I
could use a temporary maskant material but I was looking for more of a high
temperature "plug" I could slide onto the tail field, do my soldering and
then pull of the plug for flux residue cleaning. Somebody on TechNet had
recommended a couple of companies who made various plug configurations but
I can't find those notes. Hope this gives you a better visual.
Dave
Rockwell Collins
Michael McMonagle
<mmcmonagle@OYOGE
OSPACE.COM> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
01/04/2006 08:13 Re: [TN] Solder "Stop the Wicking"
AM Plugs
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Michael McMonagle
<mmcmonagle@OYOGE
OSPACE.COM>
Dave,
Can you elaborate a little more as far as the type of connector?
Might dislodge some cobwebs from the 'reference library'....
Mike McMonagle
Quality Engineer
OYO Geospace
7007 Pinemont Drive
Houston, TX 77040
713-986-8650
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Tuesday, January 03, 2006 4:31 PM
To: [log in to unmask]
Subject: [TN] Solder "Stop the Wicking" Plugs
Hi TechNet! I know I have asked this question before but I either am still
having Xmas cookie withdrawals or just have not drank enough Diet Coke
today and I can't find my old notes. Can someone please direct me to a
source of "don't let the solder wick up the connector tail" plugs/boots? I
have a connector I don't want the "connector tails" to have solder on them
and need to "block" the solder wicking action with some type of plug and/or
sleeve.
TIA!
Dave Hillman
Rockwell Collins
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|