TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"Stadem, Richard D." <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 18 Jan 2006 11:24:12 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="US-ASCII"
From:
Richard Kraszewski <[log in to unmask]>
Parts/Attachments:
text/plain (59 lines)
The latter, flaking away from the outside perimeter of the hole. 

Rich K / KEDS
260.925.8719
 

-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]] 
Sent: Wednesday, January 18, 2006 11:23 AM
To: TechNet E-Mail Forum; Richard Kraszewski
Subject: RE: [TN] ImAg Flaking away

Flaking away from the perimeter of the hole (knee) or from the perimeter
of the pad around the hole? 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Wednesday, January 18, 2006 10:20 AM
To: [log in to unmask]
Subject: [TN] ImAg Flaking away

Has anyone had any issues with ImAg breaking away from the perimeter of
a PTH?  We seem to be seeing this in a tin/lead selective soldering
operation after the board has already seen 2 previous reflows.

 

Any thoughts?  

 

Rich K / KEDS

  


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2