Franklin,
Could they be trying to achieve an 80/20 Au/Sn ratio for some high temp reflow operation? I don't have any atomic mass/density info at my fingertips. I know it sounds a little off the wall. Must be a really high Tg laminate if they were.
Steve Creswick - Gentex
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Franklin Asbell
Sent: Thursday, January 05, 2006 1:58 PM
To: [log in to unmask]
Subject: [TN] Gold over Tin
Received an unusual request for quote with a fab note callout for the
following.
1. Plate 200/50 microinches SnAu (very hard)
Now I read that as 200 microinches of tin plating, followed by 50
microinches of Gold and thought to myself..huhhhh!!!
I contacted the buyer and he agreed it was quite unusual but they indeed
need gold over tin. The buyer could not explain why, so I thought I would
see if others have performed this process, and why such uncommonly mixed
coatings???
Franklin
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|