Is the XRF a two or three element detection system?
Do you have special standards created and how expensive are they.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blomberg, Rainer
(FL51)
Sent: Thursday, January 05, 2006 9:10 AM
To: [log in to unmask]
Subject: Re: [TN] Seeking Information on Test for Pb content in SnPb
finis hed component leads
Richard, Bogert,
Yes, I agree, you took the words right out of my mouth. We use the XRF
method here at Honeywell to test lead content and we have our own
equipment.
It takes about an hour per part to do the test and write the reports.
Our
middle-of-the-road machine cost about $50K. We do a lot of parts and it
is
becoming more routine since discovery of several expensive "escapes".
Finding a pure tin component finish after-the-fact became a nightmare!
> Rainer G. Blomberg
> Honeywell -Space Systems Clearwater
> Staff Production Engineer
(727) 539-5534
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard
Sent: Thursday, January 05, 2006 8:13 AM
To: [log in to unmask]
Subject: Re: [TN] Seeking Information on Test for Pb content in SnPb
finished component leads
Happy New Year, Bogert. What is your alternate plan for retirement?
There are several methods of covering this, but the most efficient
method is
XRF. You can also avoid the cost of purchasing an XRF machine by simply
outsourcing this function to one of several materials analysis labs who
perform this analysis on a regular basis. A sample of the parts are
dropshipped to the lab, and they can perform the analysis and provide
certification to you at a very reasonable cost. You would need to
perform
the cost/benefit/ROI breakdown in order to make a decision on the best
method for your business.
Quite often the component vendors will provide you this certificate for
a
small additional cost per part. This is the cheapest method if it is
available, as the test represents the largest lot.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of - Bogert
Sent: Wednesday, January 04, 2006 6:02 PM
To: [log in to unmask]
Subject: [TN] Seeking Information on Test for Pb content in SnPb
finished
component leads
January 4, 2006
Happy New Year to all you folks. Since I did not win the Million $ PA
New
Year's day lottery, I need to continue working. Hence the following
work
related item is addressed herein and I would appreciate any help on
resolving it..
Does anyone have information on a test method/test equipment that an OEM
can
use to verify, during receiving inspection, that tin-lead plated
component
leads contain the required minimum % of lead. For example, most
mil-specs
for tin-lead plated component leads require that the Pb content be a
minimum
of 3%. What testing can the OEM do do determine this either on a lot
sample
basis, or otherwise on a 100% component basis, and what are the costs
involved for the test equipment and for
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
doing the tests?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|