You have my sympathy on that one.
Your interpretation of the homogenous is correct, and do not let your
management tell you differently!!
I also spent many a trip to the Far East in a recent employment
explaining at length why a lab analysis of a complete ground up unit was
useless.
Many companies simply have no clue or do not have the money/bandwidth to
get down to the homogenous level, so sending it out to a lab is their
idea of getting the job done quickly!!
John
John Burke
Senior Manager - Operations , Optichron
[log in to unmask]
W: 510 249 5233
M: 408 515 4992
http://www.optichron.com
Profile: https://www.linkedin.com/e/fps/2665502/
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Denis Ryskamp
Sent: Tuesday, January 24, 2006 7:20 AM
To: [log in to unmask]
Subject: Re: [LF] Declaration of compliance with material analysis
Hello all
I used to have dark brown hair but now I am gray!
Am I the only one or are others experiencing companys that provide a
declaration of compliance for their product and also send a material
analysis of the sub-components which is not performed to the Homogeneous
level just the whole sub-component ground up and tested?
Management here is asking if we are misinterpreting the Homogeneous
level
compliance requirement for a product incorporated into our product.
Seems
that some products (OEM and non-OEM) purchased are tested this way. When
reviewing the sub-component analysis, for example lead may be 129 ppm.
Figuring 10% (high)of the total weight of a connector is plating where
the
lead would be found, then one could assume that at the homogeneous level
(plating) lead would be 1290 ppm which is over the limit.
Comments?
Thanks,
Denis
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]]On Behalf Of MA/NY DDave
Sent: Friday, January 20, 2006 3:13 PM
To: [log in to unmask]
Subject: Re: [LF] Exemption of OEM products.
Hi Again David, BrianE, Genny, IPC LF Listservers,
David, Lots of good notes and thinking were posted that will hopefully
help
you with your customer and will help us think through the many
situations.
Following BrianE's logic which is good, and that crazy, to me, teddy
bear
example in the Guidance documents, I thought about Large Household
Appliances and other similar future complications.
Now most of us know that the EU hopes to recover, reuse large household
appliances to reduce them going in the dump. (80% goal). YET if I have a
Gas fired range/stove, clothes washer, clothes dryer, or other major
appliance are the electrical/electronics that part of these appliances
enough to make them EEE or is the electronics/electrical portion of
these
appliances just a tag along to their prime function. I.E. the teddy bear
example used for other products. The full gas stove, with minimial
electronics except for sensing/control is probably a weaker EEE than a
talking, winking, human interacting, solar powered teddy bear.
Yours in Engineering, Dave
YiEngr, MA/NY DDave
------------------------------------------------------------------------
----
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
------------------------------------------------------------------------
----
---
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|