One slight problem with this from a practical viewpoint.
If you have 5 microns of plating on a 0.5mm pin then scrapping 1 square
metre of pins will generate 0.05 grams of plating. The laboratory we use
for testing requires a 5 gram sample, this would require the plating to
be scrapped off an area of 100 square metres.
If any one knows of a method of scrapping plating of small pins without
any contamination from the base metal please let me know.
David Gowlett
Connector Manufacture also going grey.
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Mark Austin
Sent: 24 January 2006 15:36
To: [log in to unmask]
Subject: Re: [LF] Declaration of compliance with material analysis
IMHO
It sounds to me like the connector supplier does not understand what
homogenous is. You however are understanding it correctly.
Indeed, homogenous materials (as far as ROHS is concerned) cannot be
mechanically separated. So on a connector pin, the homogenous part is
definitely the plating as this can be mechanically scrapped from the
rest of
the pin.
Mark
===== Original Message from [log in to unmask] (Leadfree Electronics
Assembly
Forum) at 24/01/06 15:20
>Hello all
>
>I used to have dark brown hair but now I am gray!
>
>Am I the only one or are others experiencing companys that provide a
>declaration of compliance for their product and also send a material
>analysis of the sub-components which is not performed to the
Homogeneous
>level just the whole sub-component ground up and tested?
>
>Management here is asking if we are misinterpreting the Homogeneous
level
>compliance requirement for a product incorporated into our product.
Seems
>that some products (OEM and non-OEM) purchased are tested this way.
When
>reviewing the sub-component analysis, for example lead may be 129 ppm.
>Figuring 10% (high)of the total weight of a connector is plating where
the
>lead would be found, then one could assume that at the homogeneous
level
>(plating) lead would be 1290 ppm which is over the limit.
>
>Comments?
>
>Thanks,
>Denis
>
>-----Original Message-----
>From: Leadfree [mailto:[log in to unmask]]On Behalf Of MA/NY DDave
>Sent: Friday, January 20, 2006 3:13 PM
>To: [log in to unmask]
>Subject: Re: [LF] Exemption of OEM products.
>
>
>Hi Again David, BrianE, Genny, IPC LF Listservers,
>
>David, Lots of good notes and thinking were posted that will hopefully
help
>you with your customer and will help us think through the many
situations.
>
>Following BrianE's logic which is good, and that crazy, to me, teddy
bear
>example in the Guidance documents, I thought about Large Household
>Appliances and other similar future complications.
>
>Now most of us know that the EU hopes to recover, reuse large household
>appliances to reduce them going in the dump. (80% goal). YET if I have
a
>Gas fired range/stove, clothes washer, clothes dryer, or other major
>appliance are the electrical/electronics that part of these appliances
>enough to make them EEE or is the electronics/electrical portion of
these
>appliances just a tag along to their prime function. I.E. the teddy
bear
>example used for other products. The full gas stove, with minimial
>electronics except for sensing/control is probably a weaker EEE than a
>talking, winking, human interacting, solar powered teddy bear.
>
>
>Yours in Engineering, Dave
>YiEngr, MA/NY DDave
>
>-----------------------------------------------------------------------
-----
>---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text
in
>the BODY (NOT the subject field): SIGNOFF Leadfree
>To temporarily stop/(start) delivery of Leadree for vacation breaks
send:
>SET Leadfree NOMAIL/(MAIL)
>Search previous postings at: http://listserv.ipc.org/archives
>Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask]
or
>847-615-7100 ext.2815
>-----------------------------------------------------------------------
-----
>---
>
>-----------------------------------------------------------------------
----
>----Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text
in
>the BODY (NOT the subject field): SIGNOFF Leadfree
>To temporarily stop/(start) delivery of Leadree for vacation breaks
send:
>SET Leadfree NOMAIL/(MAIL)
>Search previous postings at: http://listserv.ipc.org/archives
>Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask]
or
>847-615-7100 ext.2815
>-----------------------------------------------------------------------
----
>----
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
________________________________________________________________________
This e-mail has been scanned for all viruses by Star. The
service is powered by MessageLabs. For more information on a proactive
anti-virus service working around the clock, around the globe, visit:
http://www.star.net.uk
________________________________________________________________________
________________________________________________________________________
This e-mail has been scanned for all viruses by Star. The
service is powered by MessageLabs. For more information on a proactive
anti-virus service working around the clock, around the globe, visit:
http://www.star.net.uk
________________________________________________________________________
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|