I agree with Jack the dielectric properties for polyimide (/40) aren't
different enough for that to be a driving factor in its selection. The
factors that I have seen sited in the past have always been the thermo
mechanical properties - Tg and CTE. The military pushed /40 for
avionics for a long time with LCC components since the hermetically
sealed ceramic carriers matched the polyimide's CTE closer than the
FR-4's.
Jeffrey McGlaughlin, CID
Engineering Designer EAS
4-2-50 room
x-7582 Phone
(614)458-7582 Fax
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Jack
C. Olson
Sent: Wednesday, January 25, 2006 12:10 PM
To: [log in to unmask]
Subject: Re: [DC] Polyimide laminate material
Greetings,
From my experience, engineers care more about "Dielectric Constant"
than anything else, because it affects their impedance calculations.
Are your designs impedance controlled?
However, I think the relevant value on the slash sheets is item 6
(permittivity), and /24 is listed as identical to /40!
(unless you have interesting constraints, all of the other things like
arc resistance and flammability and breakdown voltage are probably
not even an issue)
Now you got me wondering....
sorry I can't help more,
Jack
"Bremer, Gary" <[log in to unmask]>
Sent by: DesignerCouncil <[log in to unmask]>
01/25/2006 10:13 AM
Please respond to
"(Designers Council Forum)" <[log in to unmask]>; Please respond to
"Bremer, Gary" <[log in to unmask]>
To
To
[log in to unmask]
cc
Subject
[DC] Polyimide laminate material
Caterpillar: Confidential Green Retain Until: 02/24/2006
Retention
Category: G90 - General Matters/Administration
The question I have is on IPC-4101/40 material as compared to
IPC-4101/24 material. Our engineering stated they chose the Polyimide
material for all the PWB designs because of superior Dielectric
properties so to make the PWBs as thin as possible. From reading the
specification sheets for both I do not see where IPC-4101/40 material
Dielectric properties except for Arc Resistance is any better than
IPC-4101/24 material. Could someone please help me out in understanding
this issue with the dielectric properties? I would like to have a
Flammability rating of V-0 if possible on the PWBs, is there a Polyimide
material that can give me this property?
Gary Bremer
Senior Manufacturing Engineer
Curtiss-Wright Controls Inc.
Embedded Computing -Subsystem
28965 Avenue Penn
Santa Clarita, CA 91355-4185
Main: 661.257.4430 extension 2170
Fax: 661.257.4782
e-mail: [log in to unmask] <mailto:[log in to unmask]>
Web: www.cwcembedded.com <http://www.cwcembedded.com>
NOTICE: This e-mail communication is private and confidential and is
intended for the addressee only. The email may only be used for
conducting business with VISTA Controls Inc., dba Curtiss-Wright
Controls Embedded Computing Subsystems. If you are not the intended
recipient, please notify us by replying to this email followed by
deleting the email and all attachments from your system. Anyone other
than the intended recipient or those with a need to know within the
recipient's organization is strictly prohibited from using, printing,
distributing or disseminating the email or any information or attachment
contained therein.
------------------------------------------------------------------------
---------
DesignerCouncil Mail List provided as a free service by IPC using
LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases
>
E-mail Archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
------------------------------------------------------------------------
---------
------------------------------------------------------------------------
---------
DesignerCouncil Mail List provided as a free service by IPC using
LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|