In concert with John, my experience has been that when a very concientious operator applies too much coating "just to be sure", the coat skins over and either air, if it's under a component, or evaproating solvents or curing byproducts as here, can't escape and form a blister under the surface especially with heated drying. If it's near a conductor, it can be a problem. In either case, it's aesthetically undesirable. Many operators and customers don't seem to realize that conformal coating is only meant to be a mil or two thick - it's not a potting. If you've got problems with it puddling, maybe it has to be applied in a couple of thin coats. But that's slower and more labor intensive - both bad concepts.
George
(State of Franklin)
>We've got a problem here, where we're hand spraying a urethane
conformal
>coat on over a rectangular inductor.
>The inductor body is a plastic tube, with potting to fill.
>The top is not always flat (sometimes concave).
>The problem is that bubbles appear in the conformal coat on the potted
>surface, sometimes right after bake and sometimes days after.
>
>Any ideas on what the root cause is and how to prevent the bubbles?
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|