How does removing pads on unused layers affect the reliability of these
small vias, if at all? Have there been any studies done?
David Ricketts
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Hodge
Sent: 01/17/2006 2:26 PM
To: [log in to unmask]
Subject: Re: [TN] <List>Re: [TN] <List>Re: [TN] Drill and plated hole
callouts
Specifying the drill size will not prevent fractured barrels or innerlayer
separation. People are designing on the edge of drill tool capability now.
Very small vias are hard to plate and get adequate copper to survive thermal
shock. Just ask for a thermally shocked cross section of the smallest via on
the panel if you need the peace of mind. JMO
At 03:11 PM 01/17/2006, you wrote:
>I do not have a problem with through-holes for component leads and
>press-fit pins be specified that way (lots of mechanical redundancy),
>but I sure have seen a lot of plated-through vias with fractured barrel
>walls and innerlayer-separation that were not properly spec'ed.
>
>
>
>Werner
>
>---------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|