Hello,
During assembly inspection, noticed that the solder joints on the 2 sided
leads for Hirose connector, MQ172-3PA do not wet well. From the datasheet,
it seems to be of phospher bronze. As I am not a chemical gal, is this the
cause as we are using Sn37/Pb63 solder with liquid flux.
Thanks in advance for your response.
Regards,
Wee Mei
---------------------------------------------------